ASTM A1088 - 13(2019) - Standard Specification for Steel, Sheet, Cold-Rolled, Complex Phase (CP), Dual Phase (DP) and Transformation Induced Plasticity (TRIP)

ASTM A1088 - 13(2019)

Standard Specification for Steel, Sheet, Cold-Rolled, Complex Phase (CP), Dual Phase (DP) and Transformation Induced Plasticity (TRIP)

Status : Current   Published : November 2019

Format
PDF

Format
HARDCOPY



1.1 This specification covers cold-rolled, complex phase (CP) grade, dual phase (DP) grade, and transformation induced plasticity (TRIP) grade steel sheet in coils and cut lengths.

1.2 Product furnished under this specification shall conform to the applicable requirements of the latest issue of Specification A568/A568M, unless otherwise provided herein.

1.3 The product is available in a number of designations and grades with mandatory chemical requirements and mandatory mechanical properties that are achieved through thermal or thermal-mechanical treatments, and are designed to be compatible with automotive application requirements.

1.4 The grade designation nomenclature of the product differs from other cold-rolled sheet products having mandatory mechanical properties in that ordering is to tensile, rather than yield strength values.

1.5 The text of this specification references notes and footnotes that provide explanatory material. These notes and footnotes, excluding those in tables and figures, shall not be considered as requirements of this specification.

1.6 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.

1.7  This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.

1.8  This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.




Standard NumberASTM A1088 - 13(2019)
TitleStandard Specification for Steel, Sheet, Cold-Rolled, Complex Phase (CP), Dual Phase (DP) and Transformation Induced Plasticity (TRIP)
StatusCurrent
Publication Date01 November 2019
Normative References(Required to achieve compliance to this standard)No other standards are normatively referenced
Informative References(Provided for Information)No other standards are informatively referenced
Descriptors &#xfeff, cold-rolled sheet, complex phase steel, dual phase steel, steel, steel sheet, transformation induced plasticity steel
ICS77.140.50
PublisherASTM
FormatA4
DeliveryYes
Pages5
File Size101 KB
Price£40.00


 Your basket
Your basket is empty

Multi-user access to over 3,500 medical device standards, regulations, expert commentaries and other documents


Develop a PAS

Develop a fast-track standardization document in 9-12 months


Worldwide Standards
We can source any standard from anywhere in the world


BSOL

The faster, easier way to work with standards